sjudd86   +1y
Hey whats up guys.. Ive been doing alot of shaving on my truck and ive got it ground down now, but im just wonder what yall are using to smooth it out... I can use bondo.. I learned VERY well from my uncle, hes the bondo king(I mean that in a bad way)lol.. But im just looking to see what you guys use.. I dont like alot of bondo, but if thats what you guys use then that whats I'll use but. any info would be great thanks
TCFabrication   +1y
For your door handles and other places you shaved start out with Marglass or some people call it kitty hair. Spread that over your metal work and sand with 36 grit. The purpose of this is that Marglass is waterproof so it will not let moisture in through the back of your panels. After you do that use Rage Gold (thats what I like) sand that with 36 grit too. If you you have any high spots in your metal tap them down lightly. Then finish it with a glaze putty I like EverCoat metalglaze sand that with 80 grit and when you have it all featured out run over it with 180 grit and prime.
1los10   +1y
^^^ yep thats how i do it and u might hit it with a DA with 320 grit befor u prime it just to get the 180 scars out
sjudd86   +1y
thanks fellas